Fracture Resistant and Wear Corrosion Performance of CrN/ZrN Bilayers Deposited onto AISI 420 Stainless Steel
CrN/ZrN (1, 8, 15, and 30) bilayers were deposited onto AISI 420 steel substrates at 250 °C and 6.6x10-3 mbar with gas ratio Ar/N2 50:3.0 as gas mixture and ...
15 citationsDOI: https://doi.org/10.4028/www.scientific.net/amr.38.63